Interior wall tile laying process and matters needing attention

Paving of interior wall tiles is a technical activity. There are strict procedures and process requirements and should be completed by a professional construction team. The paving technology is to look at the master's technology, the owners can not ignore this link renovation. Next, we will introduce the eight steps of interior wall tiles.

1. Wall leveling. Pre-paved walls must be leveled, measured before construction, and leveled or angled and dimensionally offset walls should be leveled with cement mortar.

2, wall waterproof pretreatment. For the parts that need contact with water, water repellent agent should be used for water repellent treatment first, and then the bottom layer scraped with 1:3 cement mortar. The bottom layer should be smooth, but it should not be too smooth, until the bottom layer has 70% dryness (1-2 Day), you can lay out the construction.

3, tile soaking pretreatment. Soak the selected ceramic tiles in clean water in advance for more than 1 hour, then dry them in a vertical position. For the same wall, use a batch of soaked tiles as much as possible to avoid color differences.

4, the ground elevation. To accurately measure the elevation of the ground, make a mark and correct the ground level with cement mortar or other material (such as a turn or wood).

5, line preview. After the bottom of the wall elevation is processed, according to the size of the ceramic tile and the way of rowing the bricks, the horizontal and vertical brick centerline will pop up on the wall. Generally, the centerline of the brick is first lined up from the position of the sunken angle, and the non-complete bricks are arranged as inconspicuous as possible. Position (such as the position of the inside corner), and insert a wooden peg marked with a good paving thickness or place vertical and horizontal lines as a mark every 1-2 meters.

6, deployment of cement mortar. Use 300-grade cement, adjust to 1:1.5 suitable moisture for cement mortar, or add 5% of 107-glue pure cement slurry. Sand should be fine sand, particles should not be too thick, otherwise it will affect the viscosity or the flatness of the shop.

7, tiling. Wipe the cement mortar on the back of the tile evenly, align the drawing line and paste it on the wall, then use a rubber hammer or a small wooden hammer to tap evenly, so that the thickness of the brick surface is the same as the thickness of the wooden nail or the thickness of the vertical and horizontal line marks. For tile size errors that cause brick seam differences, apply small wood chips or toothpick or special tool pads to secure.

8, pointing. The inner wall tiles are generally used for seamless paving, and the tiles should be prevented from shifting due to cement. There is a grout that overflows the brick surface and is wiped clean with a rag after four hours. For non-edging bricks, due to the dimensional error of the bricks, it will cause about 1mm mortar joints. You can use sleek bamboo sticks to grind white grout or special sealant and evenly fill it up. Then use a special tool to make joints. The grout is even with the bricks.

Tile tile paving cement tile adhesive

Outdoor Kitchen Cabinets

Outdoor Kitchen Cabinets,Kitchen Stone Benchtops,Custom Glass Door Cabinet,Glass Door Cabinet Kitchen

PRO CABINET SOLUTION PTY LTD , https://www.pcscabinet.com.au